I crushed some Moretti Glass Rod 153022 and sprinkled on to pre-fired enamel. the bottom coat is copper flux and various colours fired by layers. I found that using glass frits brings an excellent effect on enamel firing... it's experimental work i'll
I crushed some Moretti Glass Rod 153022 and sprinkled on to pre-fired enamel. the bottom coat is copper flux and various colours fired by layers. I found that using glass frits brings an excellent effect on enamel firing... it's experimental work i'll test other frits and let you know later.
I crushed some Moretti Glass Rod 153022 and sprinkled on to pre-fired enamel. the bottom coat is copper flux and various colours fired by layers. I found that using glass frits brings an excellent effect on enamel firing... it's experimental work i'll
... moreNovember 20, 2012- -
-
Report
What technique did you use with this dish? Did you use separation enamel?
November 20, 2012- -
-
Report