I want to make champleve gold bracelet. How thick must be the 18K gold if I want 0,5-0,7mm depth enamel on top and don´t want to use counter enamel. Can I use 22K gold with better results? Is there any ratio/coefficient for gold/enamel, silver/ename...
I'm having a very hard time firing pink colors when I do cloisonne pieces. The pinks often turn orange. I've used Ninomiya L94 (raspberry), G703A, N14, SL5, and a Thompson leaded color called Tea rose. I can get a pink initially but in the final fir...
Please clear up for me what the difference is between eutectic and IT solders. I bought eutectic solder for soldering under enamel, but have since been told to use IT solder. I can find very little information about IT solder. I trust th...