  • Member
    January 9, 2015

    That the temperature in the back part of the furnace is 50 to 100 degrees Celsius higher than in the front part is normal. If the workpiece over the entire depth of the muffle ranges, you have to rotate the pieces during the firing once horizontally by 180 degrees.

    Edmund

  • Member
    January 9, 2015

     Thank you so much.